because of nitridation,the tensile strengths of 316 L and 304 L sintered in dissociated ammonia was much higher than that in vacuum,while elongation was rather lower.

 
  • 由于氮的滲入,分解氨氣氛燒結的抗拉強度比真空燒結時(shí)高出很多,但延伸率卻低了很多。