The titanium castings could be immerged into 1mol:5mol (HF:HNO 3) acid combination for 60sec after 90sec sandblasting at the pressure of 0.6 MPa in order to get rid of the whole thickness of contaminated layer of its surface.

 
  • 經(jīng) 0 .;6MPa壓力噴砂 90sec的試件在 1mol:5mol(HF :HNO3)混合酸溶液中浸泡 6 0sec即可將表面污染層完全去除