The thermal barrier coatings (TBC),which Ni30Cr12Al0.3Y bond coating was deposited by magnetron sputtering and ZrO 2 ceramic top coating was deposited by electron beam-physical vapor deposition (EB-PVD),was produced on Ni-base superalloy.
英
美
- 在Ni基單晶高溫合金基體上 ;采用磁控濺射沉積Ni30Cr12Al0 .;3Y粘結層;電子束物理氣相沉積 (EB -PVD)氧化鋯陶瓷面層;制備了熱障涂層