The superalloy GH742y prepared by spray forming were forged with forging ratio 45% by 1 250 t water press after HIP-ed.

 
  • 用噴射沉形工藝制備的GH742y合金沉積坯,經(jīng)過(guò)熱等靜壓,在1 250 t水壓機上進(jìn)行變形量為45%25的鐓餅成形。