The fracture failure reasons of the hand-gear were analyzed by means of stress situation and fractography.

 
  • 通過(guò)研究斷裂時(shí)的應力狀況及宏觀(guān)斷口,對手動(dòng)小齒輪斷裂失效原因進(jìn)行了分析。