The fracture appearances transfer from dimple to intercrystalline fracture with the temperature drops and cleavage fracture appear when work hardening happened.

 
  • 沖擊斷口由室溫下的韌窩斷口逐漸轉化為低溫下的沿晶斷口,在加工硬化時(shí)還會(huì )出現解理斷口。