The formation and aggravation of hydrogen damage in Fe-3wt-%Si alloy during cathodic charging were studied by means of Lange transmission X-ray topography.

 
  • 采用Lange式透射X射線(xiàn)形貌照相法研究了電解充氫導致Fe-3wt-%25Si單晶中氫損傷的規律。