The effect of melt superheating treatment on the microstructure and stress rupture properties of M963 superalloy under the condition of 1248 K/225 MPa has been investigated.

 
  • 對M963合金熔體進(jìn)行了過(guò)熱處理并在1248 K/225 MPa條件下測試了其持久性能.