The effect of cyclic stress on the strength of creep rupture and recurrent creep rupture as well as low cycle fatigue of a cast nickel-base superalloy with high Al and Ti contents has been studied under different temperature and stress.

 
  • 本文對一種高鋁鈦鎳基鑄造合金,在不同溫度分別測定單調持久、周期持久和低周疲勞性能。