The cyclic creep tests of a Nickel-base superalloy has been conducted on a High Temperature Electrical Creep Machine equipped with an External Digital Controler (EDC).

 
  • 本文利用裝配有EDC數字控制器的高溫電子蠕變試驗機開(kāi)展了一種鎳基高溫合金的循環(huán)蠕變實(shí)驗。