The causes of producing fine during ferromanganese-silicon cooling and crushing is analyzed. The measures and methods are put forward to prevent and reduce degradation index during crushing.

 
  • 對錳硅合金冷凝及破碎為規格粒度過(guò)程中產(chǎn)生粉末的原因進(jìn)行了分析,提出了防止和降低破粉率的措施和方法。