Microstructure and fractography for the specimens of X80 pipeline steel chargied with hydrogen in constant load tests and in slow strain rate tests(SSRT)were studied by optical microscopy and SEM.

 
  • 用光學(xué)顯微鏡和掃描電鏡觀(guān)察了不同充氫電流下恒載荷拉伸試樣、慢應變速率拉伸試樣的顯微組織和斷口形貌。