For sinter with 25% and 50% MAC fines the iron oxides mainly consisted of hematite and magnetite, the bonding phase were mainly dicalcium silicate, glassiness, and a few amount of calcium ferrite.

 
  • 配比為25%25和50%25的兩種燒結礦中鐵氧化物均以赤鐵礦、磁鐵礦為主,粘結相主要以鐵酸鈣、硅酸二鈣和玻璃質(zhì)為主,但鐵酸鈣數量不多。